Home » Boiler Tube Failure Handbook » Holes, Pits, Gouges » Fireside » Thinning from the fireside, pockmarks on external surface
Thinning from the fireside, pockmarks on external surface
Click on images to enlarge.
Comments
Corrosion associated with acidic deposits from sulfur in the fuel.
Issue Type:
Fireside » Holes, Pits, GougesLocations:
WaterwallBoiler Type:
Power (oil and natural gas fired)Industry:
Electric UtilityMechanism:
Fireside Corrosion
Download a PDF
Thinning from the fireside, pockmarks on external surface